P U Resin
SPECIFICATION
| Yes | Meets |
| Polyurethane | 1.69 |
| 1.23 | 24000 |
| 230 | 4000 |
| 5.52:1 | 4.01:1 |
| 50 mins | mins |
| 3 Hours | hours Black Brown |
| Dry Conditions: Above 15ºC, Below 35ºC | months |
| < 35ºC | 1% |
PHYSICAL PROPERTIES
| Thermal Conductivity (W/mK) | 0.35 |
| Cured Density (g/ml) | 1.60 |
| Temperature Range (°C) | -50 to +120 |
| Max Temperature Range (Short Term °C / Mins) | +125 |
| Dielectric Strength (kV/mm) | 14 |
| Volume Resistivity (ohm-cm) | 10 14 |
| Shore Hardness | A85 |
| Colour (Mixed System) | Black |
| Flame Retardency | No |
| Loss Tangent @ 50 Hz | 0.14 |
| Permittivity @ 50 Hz | 5.00 |
| Comparative Tracking Index | Not Measured |
| Water Absorption (9.7mm thick disk, 51mm diameter) | < 0.5% / < 1% |
| 10 days @ 20ºC / 1 hour @ 100ºC Elongation At Break |
Not Measured |